Young's modulus | 2525 | MPa |
Tensile strength | 50 | MPa |
Elongation | 22.5 | % |
Compressive strength | 77.5 | MPa |
Bending strength | 77.5 | MPa |
Hardness | 74 | Shore |
Yield strength | 40 | MPa |
Thermal expansion | 85 | E-6/K |
Specific heat | 1300 | J/kg*K |
Glass temperature | 115 | °C |
Minimum service temperature | -20 | °C |
Maximum service temperature | 100 | °C |
Density | 1055 | kg/m3 |
Resistivity | 1E+19 | Ohm*mm2/m |
Breakdown potential | 31 | kV/mm |
Dielectric loss factor | 0.0085 | |
Friction coefficient | 0 | |
Shrinkage | 0.55 | % |
Water absorption | 0.23 | % |